Metal working oils
Our metal working oils are produced to match to processing method based on our knowledge acquired from our long experience. Not only boosting yields but also extending the life of the dies are expected from our products. We recommend non-chlorinated type in terms of environmental protection.
The following products are typical oils. We can suggest oils matched to your processing conditions.
Environmentally friendly developed products
These metal processing oil has developed in consideration of customer's needs and the environment (non-chlorinated oil, alternative to chlorinated oil).
►Characteristics / Uses◄ | ►The leading products◄ |
Alternative to chlorinated oil / Low viscosity / Easy to be degreased / Processing of steel, SUS plate, especially for fine blanking |
►DS-71 |
Alternative to chlorinated oil / Low viscosity / Easy to be degreased / Processing of steel, SUS, aluminiumu plate for drawing or punching |
►DS-75 |
Alternative to chlorinated oil / Developed for fine blanking / Various processing of processing-difficultly materials such as SUS |
►DS-88 |
product name |
Kinematic viscosity (40℃,mm2/s) |
Extreme pressure test (Four-ball, SODA method, MPa) |
Coefficient of friction |
Flash point (℃) |
DS-71 | 17 | 0.785 | <0.115 | >130 |
DS-75 | 10 | 0.588 | <0.130 | >130 |
DS-88 | 250 | >1.471 | <0.110 | >200 |
►Others◄ | DS-12 | (Volatile / Continuous punching of Al) | DS-15K | (Low viscosity / Processing of Al) |
DS-30A | (Low viscosity / Deep-drawing of steel) | DS-72A | (Low viscosity・Bending of SUS) | |
DS-76 |
(Low viscosity / corrosion Inhibition of Cu) |
DS-86H | (High flash point) | |
Hidraw L-151 |
(Low viscosity / Deep-drawing of Al |
Water-insoluble type (non-chlorinated oil type)
►Characteristics / Uses◄ | ►The leading products◄ | |
Low viscosity / Good rust privention / Easy to be degreased General processing or drawing of steel, aluminium plate |
►DS-720 |
►Hidraw L-150 |
High viscosity / Deep-drawing of steel, aluminium plate Bending of thick plate |
►DS-771 | |
High viscosity / Good rust privention / Deep-drawing of steel plate | ►DS-775 | |
Good extreme pressure, rust prevention, lubricity / Easy to be degreased General or deep-drawing |
►PCL-227 |
product name |
Kinematic viscosity (40℃,mm2/s) |
Extreme pressure test (Four-ball, SODA method, MPa) |
Coefficient of friction |
Flash point (℃) |
DS-720 | 12 | 0.539 | <0.130 | >140 |
Hidraw L-150 | 65 | 0.588 | <0.130 | >180 |
DS-771 | 800 | 0.932 | <0.100 | >200 |
DS-775 | 373 | 0.588 | <0.125 | >180 |
PCL-227 | 56 | 0.637 | <0.120 | >150 |
Quick-volatile type (non-chlorinated oil type)
►Characteristics / Uses◄ | ►The leading products◄ | |
Thin oil film remains / Less dies-wearing / Rust prevention For continuous punching of thin steel plate |
►SY-7D | |
Carbonless or ashless after annealing Thin oil film remains / Almost not leave oil / Rust prevention For hole-punching or bending of thin plate |
►SY-10S | |
Carbonless or ashless after annealing Thin oil film remains / Rust prevention For continuous punching of thin plate, hole-punching or bending of aluminium plate |
►SY-20S | |
Quick-volatile / Blending extreme pressure For punching and forming, continuous punching. |
►SY-104 | |
Quick-volatile / Degreasing is unnecessary after processing / For processing of thin plate |
►SY-10T | ►SY-300 |
product name |
Kinematic viscosity (40℃,mm2/s) |
Coefficient of friction |
Flash point (℃) |
SY-7D | 1.07 | <0.140 | >40 |
SY-10S | 1.06 | <0.160 | >40 |
SY-20S | 0.97 | <0.160 | >40 |
SY-104 | 0.96 | <0.140 | >40 |
SY-10T | 0.89 | <0.125 | >40 |
SY-300 | 0.88 | <0.150 | >40 |
Water-soluble type (non-chlorinated oil type)
►Characteristics / Uses◄ | ►The leading products◄ |
White paste, emulsifying oil / use by diluting with water The rust is difficult to occur after machining and Degreasing is relatively easy. Processing of Aluminium plate, vessel, Consumer electronics parts |
►DS-300 |
White paste, emulsifying oil / Use by diluting with water The rust is difficult to occur and Degreasing is relatively easy. Processing of automobile and electrical parts |
►DS-303 |
Metal working oil emulsified the special wax / Use by diluting with water Hard waxy film by drying remains / Processing of steel plate, alminium |
►DS-306 |
Adding solid lubricants to water-soluble oil, emulsifying oil / Use by diluting with water Applicable to steel plate adhering oil / Applicable to steel plate which oil is adhered. |
►Superdraw #5000 |
product name |
Diluting magnification |
pH |
Extreme pressure test (Four-ball, SODA method, MPa) |
Coefficient of friction |
DS-300 | 2-7 | 8.0-9.0 | 0.588 | <0.120 |
DS-303 | 2-7 | 8.4-9.4 | 0.785 | <0.110 |
DS-306 | 2-7 | 8.0-9.0 | >1.471 |
<0.110 |
Superdraw#5000 | 2-7 | 8.5-9.5 | 0.981 | <0.110 |
Application table
The following table show some applications classified by actual example. There may be differences depending on various conditions.
Water-insoluble type and quick-volatile type
Material Processing method |
Carbon steel plate | Surface treated steel plate | Stainless | Aluminium plate |
General processing |
DS-720 Hidraw L-150 PCL-227 |
DS-720 Hidraw L-150 PCL-227 |
DS-71 DS-75 DS-76 DS-88 |
DS-74B DS-75 |
General drawing |
DS-720 Hidraw L-150 PCL-227 DS-71 |
DS-771 |
DS-71 DS-88 |
DS-771 DS-74B DS-75 |
Deep-drawing |
DS-775 DS-71 DS-74B DS-88 |
DS-771 DS-71 DS-74B DS-88 |
DS-74B DS-88 |
DS-771 DS-74B DS-75 |
Punching of thin plate |
SY-7D SY-10S SY-20S SY-300 |
SY-7D SY-10S SY-20S SY-300 |
SY-104 | SY-10S |
Punching of thick plate
|
DS-88 | DS-88 | DS-88 | ― |
Water-soluble type
Material Product name |
Carbon steel plate | Surface treated steel plate | Stainless | Aluminium plate |
DS-300 | 〇 | 〇 | 〇 |
〇 |
DS-303 | 〇 | 〇 | 〇 |
△ |
DS-306 | 〇 | 〇 | 〇 |
〇 |
Superdraw #5000 |
〇 | 〇 | 〇 | △ |